Publication date: Available online 27 November 2017
Source:Dental Materials
Author(s): Ting Khee Ho, Julian D. Satterthwaite, Nikolaos Silikas
ObjectiveTo assess the change in surface roughness of nanohybrid resin composite (Tetric EvoCeram) after antagonist wear against monolithic zirconia and lithium disilicate ceramics through a simulated chewing test using a three-dimensional (3D) profilometer.MethodsA total of 40 Tetric EvoCeram™ resin composite specimens against either a Lava™ Plus zirconia antagonist (n=20) or IPS e.max Press lithium disilicate antagonist (n=20) were prepared for the study. The surface roughness profiles of each resin composite before and after an in-vitro simulated chewing test were analysed using a 3D profilometer and Talymap software. After the simulated chewing, the surface profiles of representative Tetric EvoCeram specimens from each group were analysed using scanning electron microscopy. Independent t-test and paired t-test were used for statistical analysis.ResultsFor both lithium disilicate and zirconia groups, all surface roughness parameters (Ra, Rt, Sa, Sq,) of Tetric EvoCeram were significantly higher post-chewing compared to pre-chewing (p<0.05); the post-chewing surface roughness parameters of Tetric EvoCeram for the lithium disilicate group were significantly higher (p<0.05) than in the zirconia group.SignificanceThis chewing simulation test showed that Tetric EvoCeram composites exhibited a rougher surface when opposing lithium disilicate ceramic compared to opposing zirconia ceramic.
http://ift.tt/2zxrNhR
Medicine by Alexandros G. Sfakianakis,Anapafseos 5 Agios Nikolaos 72100 Crete Greece,00302841026182,00306932607174,alsfakia@gmail.com,
Ετικέτες
Εγγραφή σε:
Σχόλια ανάρτησης (Atom)
-
Summary Insulinomas are rare neuroendocrine tumours that classically present with fasting hypoglycaemia. This case report discusses an un...
-
The online platform for Taylor & Francis Online content New for Canadian Journal of Remote Sen...
Δεν υπάρχουν σχόλια:
Δημοσίευση σχολίου